Product Description:

HASTELLOY® G-35® RTW™ filler metal is used for the gas metal and gas tungsten arc welding of G-35® alloy. The weld metal has outstanding corrosion resistance to “fertilizer-grade” phosphoric acid, other oxidizing acids, alkalis, and chloride-bearing media. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.

Specifications:

AWS A5.14 ERNiCrMo-22    UNS N06035

Composition:

Nickel: Balance
Chromium: 32.25-34.25
Iron: 2.00 max.
Molybdenum: 7.60-9.00
Cobalt: 1.00 max.
Tungsten: 0.60 max.
Titanium: 0.20 max.
Vanadium: 0.20 max.

 

Manganese: 0.30 max.
Silicon: 0.50 max.
Other: 0.60 max.
Phosphorus: 0.03 max.
Carbon: 0.05 max.
Sulfur: 0.015 max.
Aluminum: 0.40 max.
Niobium + Tantalum 0.50 max.

Minimal Mechanical Properties:

Tensile (psi) 85,000
Mpa 590
Elongation (%) -

Available Product Forms and Sizes:

Diameter in 0.030 0.031 0.035 0.039 0.045 0.047 0.062 0.078 0.093 *0.125 *0.156x 0.187x
Diameter mm 0.76 0.80 0.89 1.00 1.10 1.20 1.60 2.00 2.40 *3.20 *4.00x *4.70x

Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.

*Size not available in MIG spools.

˟Size not available on reels.

Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.