ULTIMET® Coated Electrodes

Product Description:

ULTIMET® X coated electrodes are used for the shielded metal arc welding of ULTIMET® alloy. The deposit weld metal has exceptional resistance to galling, cavitation erosion, slurry erosion, liquid droplet impact, and various forms of corrosive attack. ULTIMET® alloy exhibits superior weldability and may be used to weld overlay carbon and stainless steels to improve their resistance to corrosion-wear. The deposit can be made easily without experiencing cracking issues common to competing alloys.

Specifications:

HAYNES PS-6041-1

Composition:

Cobalt: Balance
Chromium: 23.50-27.50
Nickel: 7.00-11.00
Molybdenum: 4.00-6.00
Iron: 1.00-5.00
Tungsten: 1.00-3.00
Manganese: 0.10-1.50

Silicon: 0.05-1.00
Other: 0.50 max.
Nickel: 0.03-0.14
Carbon: 0.02-0.10
Phosphorus: 0.030 max.
Sulfur: 0.020 max.

Minimum Mechanical Properties:

Tensile (psi)
Mpa
Elongation (%)

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150