MULTIMET® Coated Electrodes
Product Description:
MULTIMET® coated electrodes are used for the shielded metal arc welding of HAYNES® HR-120® alloy. The electrodes are also a great candidate for dissimilar joining of other high-temperature materials including HAYNES® 556® alloy, HAYNES® HR-160® alloy and other nickel and cobalt high-temperature alloys. The coating is designed for great operability, especially in out-of-position welding.
Specifications:
AMS 5795
Composition:
Iron: | Remainder |
---|---|
Chromium: | 20.0-22.5 |
Nickel: | 19.0-21.0 |
Cobalt: | 18.5-21.0 |
Molybdenum: | 2.5-3.5 |
Tungsten: | 2.0-3.0 |
Manganese: | 1.0-2.5 |
---|---|
Columbium + Tantalum | 0.75-1.25 |
Silicon: | 1.0 max. |
Carbon: | 0.10 max. |
Phosphorus: | 0.04 max. |
Sulfur: | 0.03 max. |
Minimal Mechanical Properties:
Tensile (psi) | 90,000 |
---|---|
Mpa | 620 |
Elongation (%) | 20 |
Available Product Forms and Sizes:
Diameter in | 0.093 | 0.125 | 0.156 | 0.187 |
---|---|---|---|---|
Diameter mm | 2.40 | 3.20 | 4.00 | 4.70 |
Length in | 10 | 14 | 14 | 14 |
Length mm | 254 | 355.6 | 355.6 | 355.6 |
Package Weight lbs. | 5 | 10 | 10 | 10 |
Current (A) DCEP | 40-70 | 70-100 | 80-140 | 120-150 |