HAYNES® Waspaloy RTW™ Filler Metal
Product Description:
HAYNES® Waspaloy RTW™ filler metal is used for the gas tungsten arc and gas metal arc welding of Waspaloy alloy. The deposited weld metal has excellent strength in the 1000°F-1800°F temperature range. The alloy is most commonly used for critical gas alloy turbine engine components. The RTW™ filler metal finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.
Specifications:
AMS 5828
Composition:
Nickel: | Remainder |
---|---|
Chromium: | 18.00-21.00 |
Cobalt: | 12.00-15.00 |
Molybdenum: | 3.50-5.00 |
Titanium: | 2.75-3.50 |
Iron: | 2.00 max. |
Aluminum: | 1.20-1.60 |
Carbon: | 0.02-0.10 |
---|---|
Copper: | 0.10 max. |
Manganese: | 0.10 max. |
Silicon: | 0.10 max. |
Zirconium: | 0.04 max. |
Boron: | 0.003-0.010 |
Phosphorus: | 0.0010 max. |
Sulfur: | 0.010 max. |
---|
Minimal Mechanical Properties:
Tensile (psi) | – |
---|---|
Mpa | – |
Elongation (%) | – |
Available Product Forms and Sizes:
Diameter in | 0.030 | 0.031 | 0.035 | 0.039 | 0.045 | 0.047 | 0.062 | 0.078 | 0.093 | *0.125 | *0.156x | 0.187x |
---|---|---|---|---|---|---|---|---|---|---|---|---|
Diameter mm | 0.76 | 0.80 | 0.89 | 1.00 | 1.10 | 1.20 | 1.60 | 2.00 | 2.40 | *3.20 | *4.00x | *4.70x |
Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.
*Size not available in MIG spools.
˟Size not available on reels.
Standard TIG straight lengths are available in 36” (914mm) lengths. Other lengths available upon request.