HAYNES® 117 Coated Electrodes
Product Description:
HAYNES® 117 coated electrodes are used for the shielded metal arc welding of HAYNES® 617 alloy. The weld metal has excellent high-temperature strength and resistance to oxidation. The 117 alloy electrodes are also useful for making dissimilar welds between other high-temperature materials such as 600, 601 and 800. The coating is designed for great operability, especially out-of-position welding.
Specifications:
AWS A 5.11 ENiCrCoMo-1 ASME IX F-43
ASME SFA 5.11 ENiCrCoMo-1 UNS W86117
Composition:
Nickel: | Balance |
---|---|
Chromium: | 21.0-26.0 |
Cobalt: | 9.0-15.0 |
Molybdenum: | 8.0-10.0 |
Iron: | 5.0 max. |
Manganese: | 0.3-2.5 |
Niobium* + Tantalum | 1.0 max. |
*Also known as Columbium
Silicon: | 0.75 max. |
---|---|
Copper: | 0.5 max. |
Other: | 0.5 max. |
Carbon: | 0.05-0.15 |
Phosphorus: | 0.03 max. |
Sulfur: | 0.015 max. |
Minimum Mechanical Properties:
Tensile (psi) | 90,000 |
---|---|
Mpa | 620 |
Elongation (%) | 30 |
Available Product Forms and Sizes:
Diameter in | 0.093 | 0.125 | 0.156 | 0.187 |
---|---|---|---|---|
Diameter mm | 2.40 | 3.20 | 4.00 | 4.70 |
Length in | 10 | 14 | 14 | 14 |
Length mm | 254 | 355.6 | 355.6 | 355.6 |
Package Weight lbs. | 5 | 10 | 10 | 10 |
Current (A) DCEP | 40-70 | 70-100 | 80-140 | 120-150 |