HASTELLOY® G-35® Coated Electrodes
Product Description:
HASTELLOY® G-35® coated electrodes are used for the shielded metal arc welding of G-35® alloy. The deposited weld metal has outstanding corrosion resistance to “wet process” phosphoric acid, other oxidizing acids, alkalis, and chloride-bearing media. The electrodes can also be used for the overlay and cladding of carbon steels where enhanced corrosion resistance is needed.
Specifications:
AWS A 5.11 ENiCrMo-22 UNS W86035
Composition:
Nickel: | Balance |
---|---|
Chromium: | 32.25-34.25 |
Molybdenum: | 7.6-9.0 |
Iron: | 2.0 max. |
Cobalt: | 1.0 max. |
Manganese: | 0.5 max. |
Silicon: | 0.6 max. |
Carbon: | 0.05 max. |
---|---|
Copper: | 0.3 max. |
Niobium* + Tantalum | 0.50 max. |
Tungsten: | 0.60 max. |
Aluminum: | 0.40 max. |
Titanium: | 0.20 max. |
Vanadium: | 0.20 max. |
*Also known as Columbium
Phosphorus: | 0.03 max. |
---|---|
Sulfur: | 0.015 max. |
Other: | 0.50 max. |
Minimum Mechanical Properties:
Tensile (psi) | 85,000 |
---|---|
Mpa | 590 |
Elongation (%) | 25 |
Available Product Forms and Sizes:
Diameter in | 0.093 | 0.125 | 0.156 | 0.187 |
---|---|---|---|---|
Diameter mm | 2.40 | 3.20 | 4.00 | 4.70 |
Length in | 10 | 14 | 14 | 14 |
Length mm | 254 | 355.6 | 355.6 | 355.6 |
Package Weight lbs. | 5 | 10 | 10 | 10 |
Current (A) DCEP | 40-70 | 70-100 | 80-140 | 120-150 |