HASTELLOY® 622 RTW™ Filler Metal
Product Description:
HASTELLOY® 622 RTW™ filler metal is used for weld overlay applications and has an enriched chemistry for outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. It has excellent resistance to oxidizing aqueous media including wet chlorine. The weld metal has excellent resistance to preferential corrosive attack in various media and thus is a great candidate for overlay and cladding of carbon steels. The alloy makes a great candidate for dissimilar welding of other nickel-chromium-molybdenum alloys and stainless steels. The RTW™ finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.
Specifications:
AWS A5.14 ERNiCrMo-10
ASME-SFA-5.14 ERNiCrMo-10
Composition:
Nickel: | Balance |
---|---|
Chromium: | 22.1-22.5 |
Molybdenum: | 14.0-14.5 |
Tungsten: | 3.25-3.5 |
Cobalt: | 2.50 max. |
Copper: | 0.50 max. |
Manganese: | 0.50 max. |
Other: | 0.50 max. |
---|---|
Vanadium: | 0.35 max. |
Silicon: | 0.08 max. |
Phosphorus: | 0.02 max. |
Carbon: | 0.015 max. |
Sulfur: | 0.010 max. |
Minimal Mechanical Properties:
Tensile Strength (psi) | 115,000 |
---|---|
Tensile Strength (MPa) | 793 |
Elongation (%) | 40 |
Available Product Forms and Sizes:
Diameter, in | 0.030 | 0.031 | 0.035 | 0.039 | 0.045 | 0.047 | 0.062 | 0.078 | 0.093 | *0.125 | *0.156x | *0.187x |
---|---|---|---|---|---|---|---|---|---|---|---|---|
Diameter, mm | 0.76 | 0.80 | 0.89 | 1.00 | 1.10 | 1.20 | 1.60 | 2.00 | 2.40 | *3.20 | *4.00x | *4.70x |
Filler metals are available in MIG spools, TIG cut lengths, reels, and coils from the above diameters.
*Size not available in MIG spools.
˟Size not available on reels.
Standard TIG straight lengths are available in 36” (914mm) lengths.
Other lengths available upon request.