Bar and Billet

Hot-Rolled Bar

Standard Sizes:

  • Diameter: 0.312”- 3.5″ (7.925- 88.9 mm)
  • Length: up to 12 feet (3.66 m)

Standard Finishes:

  • Annealed and Centerless Ground
  • Annealed and Pickled

Forged Bar

Standard Sizes:

  • Diameter: 3.75”- 9″ (95 mm – 228 mm)
  • Length: up to 12 feet (3.66 m)

Standard Finishes:

  • Annealed, Turned and Ground
  • Annealed and Pickled
  • Annealed and Turned

Round Billet

Standard Sizes:

  • Diameter: 3.75”- 14″ (95 mm – 355 mm)
  • Length: up to 12 feet (3.66 m)

Standard Finishes:

  • As-forged and Turned
  • As-forged, Turned, and Polished
  • As-forged and Ground

Round-Cornered Squares Billet

Standard Sizes:

  • Diameter: 3.75”- 14″ (95 mm – 355 mm)
  • Length: up to 12 feet (3.66 m)

Standard Finishes:

  • As-forged and Ground

Ingot

Standard Sizes:

  • Diameter up to 26” (660 mm)