HASTELLOY® B-3® alloy
N10675 (W80675)
800°F (427°C)5 800°F (427°)5 650°F (343°C)9 800°F (427°C)12 800°F (427°C)13 800°F (427°C)3 752°F (400°C)15,
#517
HASTELLOY® C-4 alloy
N06455 (W86455)
800°F (427°)6 800°F (427°C)8 650°F (343°C)3
800°F (427°C)21
800°F (427°C)20 800°F (427°C)18 800°F (427°C)7 752°F (400°C)16
#424
HASTELLOY® C-22® alloy
N06022 (W86022)
1250°F (677°C)1
Code Case 2226
1250°F (677°C)
800°F (427°C)1
Code Case
N-621-1
1250°F (677°C)5 1250°F (677°C)5 1250°F (677°C)1
800°F (427°C)21
1250°F (677°C)1
800°F (427°C)21
650°F (343°C)4 1250°F (677°C)12 1250°F (677°C)13 800°F (427°C)11 800°F (427°C)10 844°F (450°C)15,
#479
HASTELLOY® C-276 alloy
N10276 (W10276)
1000°F (538°C)3
Code Case 1924
1000°F (538°C)
800°F (427°C)7 800°F (427°C)7 1250°F (677°C)1 1250°F (677°C)1 650°F (343°C)1 1250°F (677°C)12 1250°F (677°C)13 1000°F (538°C)11 1250°F (677°C)10 844°F (450°C)15,
#400
HASTELLOY® C-2000® alloy
N06200 (W86200)
800°F (427°C)1 800°F (427°C)12 800°F (427°C)14 800°F (427°C)1 844°F (450°C)15
#539
HASTELLOY® G-30® alloy
N06030 (W86030)
800°F (427°C)5 800°F (427°C)5 800°F (427°C)2 800°F (427°C)21 650°F (343°C)4 800°F (427°C)12 800°F (427°C)14
HASTELLOY® G-35® alloy
N06035 (W86035)
800°F (427°C)1 800°F (427°C)14 800°F (427°C)1
HYBRID-BC1® alloy
N10362
800°F (427°C)1
Code Case 2648
HASTELLOY® N alloy
N10003
1300°F (704°C)17 800°F (427°C)17 650°F (343°C)17 1300°F (704°C)20 1300°F (704°C)19
ULTIMET® alloy
N31233
800°F (427°C)17

1Approved material forms: Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube
2Approved material forms: Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube, Bolting
3Approved material forms: Plate, Sheet, Bar, fittings, welded pipe/tube, seamless pipe/tube
4Approved material forms: Plate, Sheet, Bar, fittings, welded pipe/tube, seamless pipe/tube, Bolting
5Approved material forms: Plate, Sheet, Bar, Forgings, welded pipe/tube, seamless pipe/tube
6Approved material forms: Plate, Sheet, Bar, Forgings, welded pipe/tube, seamless pipe/tube, Bolting
7Approved material forms: Plate, Sheet, Bar, welded pipe/tube, seamless pipe/tube
8Approved material forms: Plate, Sheet, Bar, welded pipe/tube, seamless pipe/tube, Bolting
9Approved material forms: Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube
10Approved material forms: Plate, Sheet, Forgings, fittings, welded pipe/tube, seamless pipe/tube

11Approved material forms: Plate, Sheet, fittings, welded pipe/tube, seamless pipe/tube
12Approved material forms: Plate, Forgings, fittings, Bolting
13Approved material forms: Plate, Bar, Forgings, seamless pipe/tube, Bolting
14Approved material forms: Plate, Bar, Forgings, seamless pipe/tube
15Approved material forms: Plate, Sheet, Bar, Forgings
16Approved material forms: Plate, Sheet, Bar, Forgings, seamless pipe/tube
17Approved material forms: Plate, Sheet, Bar
18Approved material forms: Plate, Bar, seamless pipe/tube
19Approved material forms: Plate, Bar
20Approved material forms: Plate, Bolting