Recent data study for HAYNES® 282® alloy.

Apr 18, 2022, 11:44 AM by Kierstin Kaim
The Department of Energy conducted an in-depth study on effects of time, temperature, stress, and grain size on the predicted service-life of HAYNES® 282® alloy. Our alloy is approved for use in modern, power generation equipment that utilizes super-critical carbon dioxide and advanced, ultra-super-critical steam technologies. Click here for more information.