Alloy |
Density
lb./in3 (g/cm3)
|
Sheet,
Plate & Strip
|
Billet
Rod/Bar
|
Coated
Electrodes
|
Bare Welding
Rods
|
Seamless
Pipe & Tube
|
Welded
Pipe & Tube
|
Fittings |
Forgings |
DIN |
TUV |
Other |
HASTELLOY® B-3® alloy
N10675 (W80675)
|
0.333
(9.22)
|
SB 333/B 333
P=44
|
SB 335/ B335
B 472
P=44
|
SFA 5.11/ A 5.11
(ENiMo-10)
DIN 2.4696
(EL-NiMo28Cr)
F= 44
|
SFA 5.14/ A 5.14
(ERNiMo-10)
DIN 2.4695
(SG-NiMo30Cr)
F= 44
|
SB 622/B 622
P=44
|
SB 619/B 619
SB 626/B 626
P=44
|
SB 366/B366
SB 462/B 462
P=44
|
SB 564/B 564
SB 462/B 462
P=44
|
17744 No. 2.4600
NiMo29Cr
|
Werkstoffblatt 517
Kennblatt 7615
Kennblatt 7616
Kennblatt 7617
|
- |
HASTELLOY® C-4 alloy
N06455 (W86455)
|
0.312
(8.64)
|
SB 575/B 575
P=43
|
SB 574/B 574
P=43
|
SFA 5.11/
A 5.11
(ENiCRMo-7)
DIN 2.4612
(EL-NiMo15Cr15Ti)
F= 43
|
SFA 5.14/ A 5.14
(ERNiCrMo-7)
DIN 2.4611
(SG-NiMo16Cr16Ti)
F= 43
|
SB 622/B 622
P=43
|
SB 619/B 619
SB 626/B 626
P=43
|
SB 366/B366
P=43
|
|
17744 No. 2.4610
NiMo16Cr16Ti
|
Werkstoffblatt 424
Kennblatt 2666
Kennblatt 2667
Kennblatt 2665
|
NACE
MR0175
ISO 15156
|
HASTELLOY® C-22® alloy
N06022 (W86022)
|
0.314
(8.69)
|
SB 575/B 575
P=43
|
SB 574/B 574
B 472
P=43
|
SFA 5.11/ A 5.11
(ENiCrMo-10)
DIN 2.4638
(EL-NiCr21Mo14W)
F= 43
|
SFA 5.14/ A 5.14
(ERNiCrMo-10)
DIN 2.4635
(SG-NiCr21Mo14W)
F= 43
|
SB 622/B 622
P=43
|
SB 619/B 619
SB 626/B 626
P=43
|
SB 366/B366
SB 462/B 462
P=43
|
SB 564/B 564
SB 462/B 462
P=43
|
17744 No. 2.4602
NiCr21Mo14W
|
Werkstoffblatt 479
Kennblatt 4635
Kennblatt 4636
Kennblatt 4534
|
NACE MR0175
ISO 15156
ASME Code Case
No. 2226-2
Case No. N-621-1
|
HASTELLOY® C-22HS® alloy
N07022
|
0.311
(8.61)
|
- |
B 637 |
- |
- |
B 983 |
- |
- |
B 637 |
- |
- |
NACE MR0175 |
HASTELLOY® C-276 alloy
N10276 (W10276)
|
0.321
(8.89)
|
SB 575/B 575
P=43
|
SB 574/B 574
B 472
P=43
|
SFA 5.11/ A 5.11
(ENiCrMo-4)
DIN 2.4887
(EL-NiMo15Cr15W)
F= 43
|
SFA 5.14/ A 5.14
(ERNiCrMo-4)
DIN 2.4886
(SG-NiMo16Cr16W)
F= 43
|
SB 622/B 622
B 983
P=43
|
SB 619/B 619
SB 626/B 626
P=43
|
SB 366/B366
SB 462/B 462
P=43
|
SB 564/B 564
SB 462/B 462
P=43
|
17744 No. 2.4819
NiMo16Cr15W
|
Werkstoffblatt 400
Kennblatt 320
Kennblatt 319
|
NACE MR0175
ISO 15156
|
HASTELLOY® C-2000® alloy
N06200 (W86200)
|
0.307
(8.58)
|
SB 575/B 575
P=43
|
SB 574/B 574
B 472
P=43
|
SFA 5.11/ A 5.11
(ENiCrMo-17)
DIN 2.4699
(EL-NiCr23Mo16Cu)
F= 43
|
SFA 5.14/ A 5.14
(ERNiCrMo-17)
DIN 2.4698
(SG-NiCr23Mo16Cu)
F= 43
|
SB 622/B 622
P=43
|
SB 619/B 619
SB 626/B 626
P=43
|
SB 366/B366
SB 462/B 462
P=43
|
SB 564/B 564
SB 462/B 462
P=43
|
17744 No. 2.4675
NiCr23Mo16Cu
|
Werkstoffblatt 539
Kennblatt 9679
Kennblatt 9678
Kennblatt 9677
|
NACE MR0175
ISO 15156
|
HASTELLOY® G-30® alloy
N06030 (W86030)
|
0.297
(8.22)
|
SB 582/B 582
P=45
|
SB 581/B 581
B 472
P=45
|
SFA 5.11/ A 5.11
(ENiCrMo-11)
F= 45
|
SFA 5.14/ A 5.14
(ERNiCrMo-11)
F= 45
|
SB 622/B 622
P=45
|
SB 619/B 619
SB 626/B 626
P=45
|
SB 366/B366
SB 462/B 462
P=45
|
SB 462/B 462
P=45
|
No. 2.4603
NiCr30FeMo
|
- |
NACE MR0175
ISO 15156
|
HASTELLOY® G-35® alloy
N06035
|
0.297
(8.22)
|
SB 575/B 575
P=43
|
SB 574/B 574
B 472
P=43
|
SFA 5.11/ A 5.11
(ENiCrMo-22)
F= 43
|
SFA 5.14/ A 5.14
(ERNiCrMo-22)
F= 43
|
SB 622/B 622
P=43
|
SB 619/B 619
SB 626/B 626
P=43
|
SB 366/B366
SB 462/B 462
P=43
|
SB 564/B 564
SB 462/B 462
P=43
|
No. 2.4643
NiCr33Mo8
|
- |
NACE MR0175
ISO 15156
|
HYBRID-BC1® alloy
N10362
|
0.319
(8.83)
|
B 575
P=43
|
B 574
B 472
P=43
|
- |
ASME
Code Case
No. 2653
|
B622
P=43
|
B 619
B 626
P=43
|
B 366
P=43
|
B 462
B 564
P=43
|
No. 2.4708
NiMo22Cr15
|
- |
NACE MR0175
ISO 15156
|
HASTELLOY® N alloy
N10003
|
0.320
(8.86)
|
AMS 5607
SB 434/B 434
P=44
|
AMS 5771
SB 573/B 573
P=44
|
- |
SFA 5.14/ A 5.14
(ERNiMo-2)
F= 44
|
- |
- |
SB 366/B366
P=44
|
AMS 5771 |
- |
- |
Mil-N24390B |
ULTIMET® alloy
R31233
|
0.306
(8.47)
|
SB 818/B 818 |
B 815 |
- |
- |
- |
- |
- |
- |
No. 2.4681
CoCr26Ni9Mo5W
|
- |
NACE MR0175/MR0103
ISO 15156
|