HAYNES® 182 Coated Electrodes

Product Description:

HAYNES® 182 coated electrodes are used for the shielded metal arc welding of 600 and 601 alloys. The weld metal has good resistance to corrosion and excellent high-temperature strength and oxidation resistance. The 182 electrode is a good candidate for dissimilar joints between HAYNES® and HASTELLOY® alloys joined to stainless steels. The electrode coating has outstanding operability, especially in out-of-position welding.

Specifications:

AWS A 5.11 ENiCrFe-3            ASME IX F-43
ASME SFA 5.11 ENiCrFe-3     UNS W86182

Composition:

Nickel: Balance
Chromium: 13.0-17.0
Cobalt: 0.12 max.*
Titanium: 1.0 max.
Iron: 10.0 max.
Manganese: 5.0-9.5
Niobium** + Tantalum 1.0-2.5

*When specified by customer
**Also known as Columbium

 

Silicon: 1.0 max.
Copper: 0.5 max.
Other: 0.5 max.
Carbon: 0.1 max.
Phosphorus: 0.03 max.
Sulfur: 0.015 max.

Minimal Mechanical Properties:

Tensile (psi) 80,000
Mpa 550
Elongation (%) 30

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150