Product Description:

HAYNES® 122 coated electrodes are used for the shielded metal arc welding of C-22®, 622, 625 and 825 alloys. The electrodes are also a good candidate for welding stainless steels that contain molybdenum for corrosion resistance. The alloy also effectively overmatches alloys 625 and C-276. The electrodes have a slag system that promotes great operability in all positions, especially out-of-position welding.

Specifications:

AWS A 5.11 ENiCrMo-10            UNS W86022
ASME SFA 5.11 ENiCrMo-10     ASME IX F-43
Kennblatt 04534.03
*Specify at time of order

Composition:

Nickel: Balance
Chromium: 20.0-22.5
Cobalt: 2.5 max.
Molybdenum: 12.5-14.5
Iron: 2.0-6.0
Manganese: 1.0 max.
Vanadium: 0.35 max.

 

Silicon: 0.2 max.
Copper: 0.5 max.
Other: 0.5 max.
Carbon: 0.02 max.
Phosphorus: 0.03 max.
Sulfur: 0.015 max.
Tungsten: 2.5-3.5

Minimal Mechanical Properties:

Tensile (psi) 100,000
Mpa 690
Elongation (%) 25

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150