HAYNES® 117 Coated Electrodes

Product Description:

HAYNES® 117 coated electrodes are used for the shielded metal arc welding of HAYNES® 617 alloy. The weld metal has excellent high-temperature strength and resistance to oxidation. The 117 alloy electrodes are also useful for making dissimilar welds between other high-temperature materials such as 600, 601 and 800. The coating is designed for great operability, especially out-of-position welding.

Specifications:

AWS A 5.11 ENiCrCoMo-1            ASME IX F-43
ASME SFA 5.11 ENiCrCoMo-1     UNS W86117

Composition:

Nickel: Balance
Chromium: 21.0-26.0
Cobalt: 9.0-15.0
Molybdenum: 8.0-10.0
Iron: 5.0 max.
Manganese: 0.3-2.5
Niobium + Tantalum 1.0 max.

 

Silicon: 0.75 max.
Copper: 0.5 max.
Other: 0.5 max.
Carbon: 0.05-0.15
Phosphorus: 0.03 max.
Sulfur: 0.015 max.

Minimum Mechanical Properties:

Tensile (psi) 90,000
Mpa 620
Elongation (%) 30

Available Product Forms and Sizes:

Diameter in 0.093 0.125 0.156 0.187
Diameter mm 2.40 3.20 4.00 4.70
Length in 10 14 14 14
Length mm 254 355.6 355.6 355.6
Package Weight lbs. 5 10 10 10
Current (A) DCEP 40-70 70-100 80-140 120-150