Specifications

Codes

HAYNES® 625 alloy
(N06625, W86112)
Sheet, Plate & Strip AMS 5599
SB 443/B 443
AMS 5869
P= 43
Billet, Rod & Bar AMS 5666
SB 446/B 446
B 472
P= 43
Coated Electrodes SFA 5.11/ A 5.11
(ENiCrMo-3)
F= 43
Bare Welding Rods & Wire SFA 5.14/ A 5.14
(ERNiCrMo-3)
AMS 5837
F=43
Seamless Pipe & Tube AMS 5581
SB 444/B 444
P= 43
Welded Pipe & Tube AMS 5581
SB 704/B 704
SB 705/B 705
P= 43
Fittings SB 366/B 366
P= 43
Forgings AMS 5666
SB 564/B 564
P= 43
DIN 17744 No. 2.4856
NiCr22Mo9Nb
Others ASME Code Case No. 2468
NACE MR0175
ISO 15156
HAYNES® 625 alloy
(N06625, W86112)
ASME Section l Grade 1
1100ºF (593ºC)1
Cold Case 2632
1200ºF (650ºC)2
Grade 2
1100ºF (593ºC)3
Code Case 1935
1000ºF (538ºC)3
Section lll Class 1 Grade 1
800ºF (427ºC)3
Class 2 Grade 1
800ºF (427ºC)4
Class 3 Grade 1
800ºF (427ºC)4
Section lV HF-300.2 -
Section Vlll Div. 1 Grade 1
1200ºF (649ºC)1
Grade 2
1600ºF (871ºC)3
1200ºF (649ºC)5
Div. 2 Grade 1
800ºF (427ºC)5
Code Case 2468
800ºF (427ºC)6
Section Xll Grade 1
650ºF (343ºC)1
Grade 2
650ºF (343ºC)7
B16.5 1200°F (649°C)8
B16.34 1200°F (649°C)6
B31.1 1200°F (649°C)1
B31.3 1200°F (649°C)6
MMPDS  6.3.3
1Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube
2Plate, Sheet, welded pipe/tube
3Plate, Sheet, Bar, seamless pipe/tube
4Plate, Sheet, Bar, Forgings, welded pipe/tube, seamless pipe/tube
5Bolting
6Plate, Sheet, Bar, Forgings, seamless pipe/tube
7Plate, Sheet, Bar, seamless pipe/tube, Bolting