phone-icon800.354.0806
765.456.6012
The Home of HASTELLOY® and
HAYNES® Alloys

Specifications and Codes

Specifications

Codes

HAYNES® HR-160® alloy
(N12160)
Sheet, Plate & Strip SB 435/B 435
P= 46
Billet, Rod & Bar SB 572/B 572
B 472
P= 46
Coated Electrodes -
Bare Welding Rods & Wire SFA 5.14/ A 5.14 (ERNiCoCrSi-1)
F= 46
Seamless Pipe & Tube SB 622/B 622
P= 46
Welded Pipe & Tube SB 619/B 619
SB 626/B 626
P= 46
Fittings SB 366/B 366
P=46 
Forgings SB 564/B 564
P= 46
DIN No. 2.4880
NiCo29Cr28Si
Others -

HAYNES® HR-160® alloy
(N12160)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 -
Section lV HF-300.2 -
Section Vlll Div. 1 1800°F (982°C)1,2
Div. 2 -
Section Xll -
B16.5 -
B16.34 -
B31.1 -
B31.3 -

1Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube
2ASME Code Case No. 2385

Print Page Download Page