phone-icon800.354.0806
765.456.6012
The Home of HASTELLOY® and
HAYNES® Alloys

Specifications and Codes

Specifications

Codes

HAYNES® 242® alloy
(N10242)
Sheet, Plate & Strip SB 434/B 434
P= 44
Billet, Rod & Bar SB 573/B 573
B 472
P= 44
Coated Electrodes -
Bare Welding Rods & Wire SFA 5.14/ A 5.14 (ERNiMo-12)
F= 44
Seamless Pipe & Tube SB 622/B 622
P= 44
Welded Pipe & Tube SB 619/B 619
SB 626/B 626
P= 44
Fittings SB 366/B 366
P= 44
Forgings SB 564/B 564
P= 44
DIN -
Others -
HAYNES® 242® alloy
(N10242)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 -
Section lV HF-300.2 -
Section Vlll Div. 1 1000°F (538°C)1
Div. 2 -
Section Xll -
B16.5 -
B16.34 -
B31.1 -
B31.3 -
1Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube