HYBRID-BC1® alloy
(N10362)
Sheet, Plate & Strip B575
P= 43
Billet, Rod & Bar B574
B472
P= 43
Coated Electrodes -
Bare Welding Rods & Wire ASME
Code Case
No. 2653
Seamless Pipe & Tube B622
P= 43
Welded Pipe & Tube B619
B626
P= 43
Fittings B366
Forgings B462
B564
P= 43
DIN No. 2.4708 NiMo22Cr15
TÜV -
Others -
HYBRID-BC1®
(N10362)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 -
Section Vlll Div. 1 800°F (427°C)1
Div. 2 -
Section Xll -
B16.5 -
B16.34 -
B31.1 800°F (427°C)1
B31.3 800°F (450°C) 
VdTÜV (doc #) -
1Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube