Specifications and Codes

Specifications

Codes

HASTELLOY® G-30® alloy
(N06030, W86030)
Sheet, Plate & Strip SB 582/B 582
P= 45
Billet, Rod & Bar SB 581/B 581
B 472
P= 45
Coated Electrodes SFA 5.11/ A 5.11 (ENiCrMo-11)
F= 45
Bare Welding Rods & Wire SFA 5.14/ A 5.14 (ERNiCrMo-11)
F= 45
Seamless Pipe & Tube SB 622/B 622
P= 45
Welded Pipe & Tube SB 619/B 619
SB 626/B 626
P= 45
Fittings SB 366/B 366
SB 462/B 462
P= 45
Forgings SB 462/B 462
P= 45
DIN No. 2.4603 NiCr30FeMo
TÜV -
Others NACE MR0175
ISO 15156
HASTELLOY® G-30® alloy
(N06030, W86030)
ASME Section l -
Section lll Class 1
Class 2
Class 3
Section Vlll Div. 1
Div. 2
Section Xll 650°F (343°C)1
B16.5 800°F (427°C)2
B16.34 800°F (427°C)3
B31.1 -
B31.3 -
VdTÜV (doc #) -
1Plate, Sheet, Bar, fittings, welded pipe/tube, seamless pipe/tube, Bolting
2Plate, Forgings, fittings
3Plate, Bar, Forgings, seamless pipe/tube