phone-icon800.354.0806
765.456.6012
The Home of HASTELLOY® and
HAYNES® Alloys

Specifications and Codes

Specifications

Codes

HASTELLOY® C-276 alloy
(N10276, W10276)
Sheet, Plate & Strip SB 575/B 575
P= 43
Billet, Rod & Bar SB 574/B 574
P= 43
Coated Electrodes SFA 5.11/ A 5.11 (ENiCrMo-4)
DIN 2.4887
(EL-NiMo15Cr15W)
F= 43
Bare Welding Rods & Wire SFA 5.14/ A 5.14 (ERNiCrMo-4)
DIN 2.4886
(SG-NiMo16Cr16W)
F= 43
Seamless Pipe & Tube SB 622/B 622
P= 43
Welded Pipe & Tube SB 619/B 619
P= 43
Fittings SB 366/B 366
P= 43
Forgings SB 564/B 564
P= 43
DIN 17744 No. 2.4819 NiMo16Cr15W
TÜV Werkstoffblatt 400
Kennblatt 320
Kennblatt 319
Others NACE MR0175
ISO 15156

HASTELLOY® C-276 alloy
(N10276, W10276)
ASME Section l 1000°F (538°C)1
Section lll Class 1 -
Class 2 800°F (427°C)2
Class 3 800°F (427°C)2
Section Vlll Div. 1 1250°F (677°C)3
Div. 2 1250°F (677°C)3
Section Xll 650°F (343°C)3
B16.5 1250°F (677°C)4
B16.34 1250°F (677°C)5
B31.1 1000°F (538°C)6
B31.3 1250°F (677°C)7
VdTÜV (doc #) 844°F (450°C)8,
#400
1Plate, Sheet, Bar, fittings, welded pipe/tube, seamless pipe/tube
2Plate, Sheet, Bar, welded pipe/tube, seamless pipe/tube
3Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube
4Plate, Forgings, fittings
5Plate, Bar, Forgings, seamless pipe/tube
6Plate, Sheet, fittings, welded pipe/tube, seamless pipe/tube
7Plate, Sheet, Forgings, fittings, welded pipe/tube, seamless pipe/tube
8Plate, Sheet, Bar, Forgings