phone-icon800.354.0806
765.456.6012
The Home of HASTELLOY® and
HAYNES® Alloys

Specifications and Codes

Specifications

Codes

HASTELLOY® C-2000® alloy
(N06200, W86200) 
Sheet, Plate & Strip SB 575/B 575
P= 43
Billet, Rod & Bar SB 574/B 574
B 472
P= 43
Coated Electrodes SFA 5.11/ A 5.11 (ENiCrMo-17)
DIN 2.4699
(EL-NiCr23Mo16Cu)
F= 43
Bare Welding Rods & Wire SFA 5.14/ A 5.14 (ERNiCrMo-17)
DIN 2.4698
(SG-NiCr23Mo16Cu)
F= 43
Seamless Pipe & Tube SB 622/B 622
P= 43
Welded Pipe & Tube SB 619/B 619
SB 626/B 626
P= 43
Fittings SB 366/B 366
SB 462/B 462
P= 43
Forgings SB 564/B 564
SB 462/B 462
P= 43
DIN 17744 No. 2.4675 NiCr23Mo16Cu
TÜV Werkstoffblatt 539
Kennblatt 9679
Kennblatt 9678
Kennblatt 9677
Others NACE MR0175
ISO 15156
HASTELLOY® C-2000® alloy
(N06200, W86200)
ASME Section l -
Section lll Class 1 -
Class 2 -
Class 3 -
Section Vlll Div. 1 800°F (427°C)1
Div. 2 -
Section Xll -
B16.5 800°F (427°C)2
B16.34 800°F (427°C)3
B31.1 -
B31.3 800°F (427°C)1
VdTÜV (doc #) 844°F (450°C)4,
#539
1Plate, Sheet, Bar, Forgings, fittings, welded pipe/tube, seamless pipe/tube
2Plate, Forgings, fittings, Bolting
3Plate, Bar, Forgings, seamless pipe/tube
4Plate, Sheet, Bar, Forgings