Nominal Composition

Weight %

Nickel: 65 min.
Molybdenum: 28.5
Chromium: 1.5
Iron: 1.5
Tungsten: 3 max.
Manganese: 3 max.
Cobalt: 3 max.
Aluminum: 0.5 max.
Titanium: 0.2 max.
Silicon: 0.1 max.
Carbon: 0.01 max.
Niobium:
0.2 max.
Vanadium:  0.2 max. 
Copper:  0.2 max. 
Tantalum:  0.2 max. 
Zirconium:  0.01 max. 