Cavitation Test |
|
ASTM Standard G 32
Frequency-20 kHz
Amplitude-0.05 mm
Liquid-Distilled Water
Test Duration-24 hr.
Room Temperature |
|
|
Slurry Test |
|
Medium-80 microns Alumina
in Tap Water
Velocity-5 m/s
Impact Angle-30°
Particle Loading-0.12 kg/l
Test Duration-40hr.
Room Temperature |
|
|
Solid Particle Test |
|
ASTM Standard G 76 (Modified)
Erodent-400 microns Angular
Silicon Carbide
Velocity-20 m/s
Impact Angle-60°
Total Flow-80g of Erodent
Room Temperature |
|
|