| For More Technical Detail Request the Following Haynes International Brochures: |
H-2087 Reference Guide for Optimum Protection Against Corrosion and Wear
H-2099 Guidelines for Weld Surfacing with ULTIMET Wire
H-2089 ULTIMET alloy Welding Guidelines
H-2086 ULTIMET alloy Machining Guidelines
H-1034 Applicable Specifications |
| ULTIMET alloy Specifications |
UNS R31233
ASTM B-815 (Rod)
ASTM B-818 (Plate, Sheet, Strip)
ASME Section VIII, Div. 1, Code Case 2121
DIN CoCr26Ni9Mo5W No. 2.4681
NACE MR-01-75 Section 4.1.6.3 |
| Available Wrought Product Forms |
Bar (>12.7 mm/0.5 in.)
Billet Standard Sizes
Plate Standard Sizes
Sheet (>1.6 mm/0.063 in.)
Wire Standard Sizes
Weld Products (GTA, GMA, SMA, SAW) |
 |
|
| Castings |
AOD Refined Master Alloy
(Remelt Bar) from
Cannon-Muskegon
Tel: 616-755-1681
Fax: 616-755-4016 |
| Powders |
Gas Atomized Powders For:
Plasma Transferred Arc (PTA) welding and
Thermal Spray Coating from
Deloro Stellite
Tel: 800-235-9353 or 574-534-2585
Fax: 574-534-3417 |
Acknowledgments:
CARPENTER and 20CB-3 are registered trademarks of Carpenter Technology Corporation
NITRONIC is a registered trademark of Armco Steel Corporation
800HT is a registered trademark of Inco Family of Companies
STELLITE is a registered trademark of Thermadyne Deloro Stellite Inc. |