Research and Technology Group
Technology Laboratories and Equipment |
|
The 100-lb vacuum induction (VIM)
furnace is used to primary melt
experimental alloys. |
|
 |
|
An air induction furnace is used to melt liquid slag for the electroslag remelting process. |
|
| The 1200-ton forge press is used to hot work 4-inch diameter electroslag remelted ingots down to a slab of about 2 inches thick. |
|
|
|
|
|
The 2-high rolling mill is used to hot roll slab down to plate or sheet. |
|
|
 |
|
| The cold rolling mill can achieve further reductions down to thin sheet gauges. |
|
|
|
|
|
|
|
A sandblasting facility is available
for
cleaning hot rolled and annealed
materials. |
|
Ancillary equipment is available for
drilling and specimen preparation.
|
|
 |
A plasma arc cutting facility equipped with an optical tracer can cut a variety of shapes from plate up to 1 1/2 inches thick. |
|
A fully equipped welding laboratory is used to prepare weldment
samples or conduct weldability evaluations.
|
|
|
|
Shielded Metal Arc Welding (SMAW) |
|
|
 |
Gas Tungsten Arc Welding (GTAW) |
|
Gas Metal Arc Welding (GMAW) |
|