A solid-solution-strengthened,
high-temperature corrosion-resistant
alloy that provides
excellent resistance
to
sulfidation and chloride attack
in both reducing and oxidizing
atmospheres with
exceptionally
good resistance to oxidation,
hot corrosion, carburization,
metal dusting, and nitridation.