| Comparative Cost of Heat-Resistant Alloys* |
| The initial premium for higher cost alloy construction is often recovered via improved equipment performance,
minimizing repair replacement and down-time and increasing throughput rates and cycle times.
Comparative costs of a wide range of heat-resistant alloys are presented below. These tabulations
represent average composits of 1991/1992 pricing information supplied by prominent alloy suppliers in
the United States...(1) |
Alloys |
Relative Cost |
304 SS |
1.00 (Basis) |
309 SS |
1.6 |
446 SS |
1.7 |
310 SS |
2.0 |
253MA, RA85H |
2.3 |
800H, 330 |
2.6-3.0 |
HR-120® |
3.5 |
600, 601 |
3.8-4.3 |
333 |
5.1 |
X |
4.8-5.6 |
556® |
8.5 |
HR-160® |
12 |
| |
|
| *1991-1992 prices/lb., 1/4-in. plate. |
| |
|
|
| 1 “Alloy Selection for Waste Incineration Facilities”, G. Sorell, 1992 Incineration Conference.
|