Temp., °F |
British Units |
Temp., °C |
Metric Units |
|
Room |
30.2 x 106 psi |
Room |
208 GPa |
200 |
29.2 x 106 psi |
100 |
201 GPa |
400 |
28.8 x 106 psi |
200 |
199 GPa |
600 |
27.7 x 106 psi |
300 |
192 GPa |
800 |
26.7 x 106 psi |
400 |
186 GPa |
1000 |
25.6 x 106 psi |
500 |
179 GPa |
1200 |
24.3 x 106 psi |
600 |
171 GPa |
1400 |
22.8 x 106 psi |
700 |
163 GPa |
1600 |
21.2 x 106 psi |
800 |
153 GPa |
1800 |
18.7 x 106 psi |
900 |
142 GPa |
- |
- |
1000 |
126 GPa |
|