Applications
Sour Gas Service |
|
|---|---|
![]() |
HASTELLOY® G-50® alloy gives good service in deep sour gas wells despite severe condition of heat and corrosion. The alloy provides reliable service in resisting a saline solution of hydrogen sulfide. |