Metal Finishing |
|
|---|---|
![]() |
HASTELLOY® G-30® alloy has outstanding resistance to nitric/hydrofluoric acid mixtures, such as those employed in the pickling of stainless steels and titanium. This G-30® alloy hook offered seven times the life of C-276 alloy in this titanium pickling environment and was available at 25% lower costs. |
|
![]() |