HAYNES® 625 alloy InformationUNS No. N06625 62Nia-21Cr-9Mo-5Fe*-3.7Cb+Ta-1Co*-0.5Mn*-0.5Si*-0.4Al*-0.4Ti*-0.10C*
|
||||
|
||||
|
|
|
| ||||
|
|
|
| ||||
|
|