TYPICAL APPLICATIONS

This horizontal electrically fired 230® retort replaced an alloy 600 retort which lasted only an average of  eight months in 1400 to 2200°F (760 to 1205°C) service in hydrogen atmosphere.  The 230 retort was still in excellent condition after 24 months service, as shown. 
Wire annealing fixture of 230 alloy reduces thermal mass and cycle times after replacing massive carbon-steel "stub" used previously.
Fabricated heat-treating basket for vacuum furnace application to 2300°F (1260°C).  Made from 1/2-inch (12.7 mm) diameter 230 bar. 
This striking shot of a HAYNES 230 heat-treat fixture was taken at a leading off-road automotive equipment plant.  This conveyor fixture operates at 1550°F (845°C) with a subsequent water quench followed by a four hour cycle at 1050°F (565°C).
 
Back to Typical Applications