TYPICAL APPLICATIONS

 
Nitric acid catalyst grids support made from HAYNES® 230® alloy plate and bar.  Excellent creep strength at 1700°F (927°C) makes the alloy highly suitable for this application.
 
Textron Lycoming gas turbine engine combustor made of HAYNES® 230® alloy.
 